This page presents the S-N curves and fatigue limit of MS1 steel samples that underwent shot-peening, heat treatment and machining that removed allowance of 4mm (in that order), obtained using the bending tests of rotating bars with AM layers normal to the axis of rotation.
| Build orientation of longitudinal axis | vertical | 
|---|---|
| Position with respect to inert gas flow | undefined | 
| Post-processing | shot-peening → heat treatment → machining allowance 4mm | 
| Fatigue limit (MPa) | 601 | 
|---|---|
| Number of cycles to failure N | N=1,48⋅10<html>31</html>⋅S<html>-8,70</html> | 
| Stress amplitude S (MPa) | S=3843⋅N<html>-0,115</html> | 
Explanation of the terms are given at the page Fatigue strength description.
This page is a part of the section DMLS/SLM: Fatigue design rules.